CuSn4Zn4Pb4 — C54400
CuSn4Zn4Pb4-C54400 free cutting phosphor bronze, C54400 phosphor bronze, CuSn4Zn4Pb4, QSn4-4-4, JIS C5441, Free bronze rod, C54400 phosphor bronze rod, ASTM C54400
Chemical Composition
| Element | Content |
|---|---|
| Sn | 3.50-4.50% |
| Pb | 3.50-4.50% |
| Zn | 3.50-4.50% |
| P | 0.01-0.50% |
| Fe | 0.10% Max. |
| Zn | Balance |
Physical Properties
| Property | Value |
|---|---|
| Specific Gravity | 8.89 g/cm3 |
| Coefficient of Thermal Expansion per °C | 17.30 x 10-6 (20-300°C) |
| Electrical Conductivity (% IACS) | 19.00 % @ 68 F |
| Thermal Conductivity | 50.00 Btu · ft/(hr · ft2·oF)at 68F |
| Modulus of Elasticity in tension | 15000 ksi |
International Specification
| Product Form | Specification |
|---|---|
| Rods/Bars | UNS.C54400, CDA544, ASTM B139, B103 |
| European Standards | CuSn4Zn4Pb4,JIS H3270, EN 12164 CW 456 K |
Where This Grade Is Used
Electrical
Industrial
Marine
Frequently Asked Questions
What is the chemical composition of C54400?
C54400 is supplied to the following nominal composition: Sn: 3.50-4.50% Pb: 3.50-4.50% Zn: 3.50-4.50% P: 0.01-0.50% Fe: 0.10% Max. Zn: Balance
What are the typical physical properties of C54400?
Typical values published by Vital for C54400: Specific Gravity: 8.89 g/cm3 Coefficient of Thermal Expansion per °C: 17.30 x 10-6 (20-300°C) Electrical Conductivity (% IACS): 19.00 % @ 68 F Thermal Conductivity: 50.00 Btu · ft/(hr · ft2·oF)at 68F Modulus of Elasticity in tension: 15000 ksi
Which international specifications does C54400 meet?
Rods/Bars: UNS.C54400, CDA544, ASTM B139, B103 European Standards: CuSn4Zn4Pb4,JIS H3270, EN 12164 CW 456 K
Can you supply mechanical property data for C54400?
The detailed Mechanical Properties will be available on request from customers.
Which product forms and sizes are available?
Custom Diameter & Sizes, Random Mill lengths Round bars, Flat bars, Square bars, Round Wires, Round Strips Custom shapes are available upon request.
How do I request a quotation?
Email the grade, temper, dimensions and quantity to [email protected] . Unless otherwise specified, material is produced to ASTM.
Quote This Grade To Your Specification
Send your requirements for CuSn4Zn4Pb4 — C54400 and we will quote against your specification.